This book addresses the need for comprehensive, advanced models that integrate the various stages and factors involved in the pitting corrosion process. It covers corrosion fatigue mechanisms and the influence of stress and temperature, and ways to mitigate corrosion induced damage in structural components. Seasonal Blurb